Ti-Zr-V-Nb-Al BCC high-entropy alloy with outstanding uniform ductility achieved by grain refinement

Figure 5. Schematic diagram of the chosen different locations (A); the dislocation density at chosen locations at 1%, 3%, 5%, 7%, 9% and 12% strains of coarse- (B) and fine-grained (C) TZ alloys. TZ: Ti-Zr-V-Nb-Al.