Figure6

Imaging inter - and intra-particle features in crystalline cathode materials for Li-ion batteries using nano-focused beam techniques at 4th generation synchrotron sources

Figure 6. Scanning X-ray nanodiffraction microscopy of NMC622 cathode single crystal. Tilt Magnitude of crystal deviation from mean direction (altitude) (A and B). Local distortion in orientation of lattice vs. mean direction (azimuth) (C and D). Crystal misorientation map (Direction $$ \cdot $$ Magnitude) (E and F). Pixel distribution of Misorientation Map projected on the 2D scatter polar plot (G and H)