fig2

Enabling highly reversible Zn anode via an interfacial preferentially adsorbed additive containing nucleophilic groups

Figure 2. (A) Contact angle measurements of different electrolytes on zinc metal foil. (B) Nucleation overpotential at 1 mA cm-2 using different electrolytes. (C) CV curves of symmetric cells in different electrolytes. CE of asymmetric cells in different electrolytes at (D) 6 mA cm-2 and (F) 2 mA cm-2. (E) Voltage profiles of Zn//Cu asymmetric cell with MA at 6 mA cm-2.