Construction and ultrasonic inspection of the high-capacity Li-ion battery based on the MnO<sub>2</sub> decorated by Au nanoparticles anode

Figure 1. (A) XRD patterns of MnO2-Au under ultrasound for 30 min (red line) and ultrasound for 20 min (black line). (B) XRD patterns of MnO2-Au under different concentration ratios of NaBH4 and HAuCl4. SEM images of MnO2-Au (C and D).