Figure 1. XRD patterns (A), the characteristic diffraction peaks of different phases (marked with different colors) and mechanical properties [Vickers’ Hardness (B) and Fracture Toughness (C)] of recovered samples sintered at 25 GPa and 500-1,800 °C, named as BNCT (T represent temperatures).