fig11
![Cryogenic atom probe tomography and its applications: a review](https://image.oaes.cc/5ca7242f-4578-410a-9002-1be3b02ceea2/microstructures3038.fig.11.jpg)
Figure 11. 3-D APT atom map and proximity histograms across the alkali-rich/alkali-poor interface in water and across the water/corroded glass interface. (A) 3-D APT atom map and proximity histograms across (B) the alkali-rich/alkali-poor interface in water and (C) across the water/corroded glass interface. Error bars indicate 1-sigma from standard counting error. Reproduced with the permission of Ref.[39] Copyright 2018, Elsevier.