fig2
![Optimizing the energy storage performance of NaNbO<sub>3</sub> ceramics by rare-earth-based composite perovskite Sm(Mg<sub>0.5</sub>Zr<sub>0.5</sub>)O<sub>3</sub> modification](https://image.oaes.cc/4b623cc5-91f8-4cb6-a3ed-f2492c1344ef/microstructures3019.fig.2.jpg)
Figure 2. Raman Test Diagram of NaNbO3-xSm(Mg0.5Zr0.5)O3 ceramics (0.05 ≤ x ≤ 0.15) (A) and the Raman vibration modes v1 (B) and v5 (C) of NN-SMZ components are plotted.
Figure 2. Raman Test Diagram of NaNbO3-xSm(Mg0.5Zr0.5)O3 ceramics (0.05 ≤ x ≤ 0.15) (A) and the Raman vibration modes v1 (B) and v5 (C) of NN-SMZ components are plotted.