fig4
![High energy storage properties of 0.94Bi<sub>0.5</sub>Na<sub>0.5</sub>TiO<sub>3</sub>-0.06BaTiO<sub>3</sub> ceramics by incorporating <InlineParagraph>Sr<sub>0.8</sub>Bi<sub>0.1γ0.1</sub>Ti<sub>0.8</sub>Zr<sub>0.2</sub>O<sub>2.95</sub></InlineParagraph>](https://image.oaes.cc/3efa2828-3ae7-482b-a9f4-65b68386516f/5729.fig.4.jpg)
Figure 4. Plots of ln(1/ε-1/εmax) as a function of ln(T-Tm) at 1 kHz by the modified Curie-Weiss law.
Figure 4. Plots of ln(1/ε-1/εmax) as a function of ln(T-Tm) at 1 kHz by the modified Curie-Weiss law.