Figure 10. Surface morphology (A-D) and the average corrosion rate (E) by mass loss of the CrxMnFeCoNi (x = 0, 0.6, 1, and 1.5) HEAs after immersion in a 0.5 M H2SO4 solution for 15 days at room temperature. HEAs: high-entropy alloys.