![Microstructure evolution in laser powder bed fusion-built Fe-Mn-Si shape memory alloy](https://image.oaes.cc/fe4cc682-a6d0-477d-b03c-07b405ca9597/5402.fig.10.jpg)
Figure 10. The relationship between residual strain (average KAM value) and hardness for both the reference alloy and the LPBF alloy fabricated at different LEDs.
Figure 10. The relationship between residual strain (average KAM value) and hardness for both the reference alloy and the LPBF alloy fabricated at different LEDs.