fig8
![BaTiO<sub>3</sub>-NaNbO<sub>3</sub> energy storage ceramics with an ultrafast charge-discharge rate and temperature-stable power density](https://image.oaes.cc/efb6495c-8b6f-4a10-8ed1-597e4de0f80e/5271.fig.8.jpg)
Figure 8. (A) Overdamped pulsed discharge current curves under various E values and (B) corresponding Wd as a function of time. Undamped pulsed discharge current curves (C) at 25 °C under various E values and (E) at 20 MV m-1 under various temperatures and (D and F) corresponding CD and PD values.