![Effects of processing parameters on a β-solidifying TiAl alloy fabricated by laser-based additive manufacturing](https://image.oaes.cc/408446ac-1c23-49cb-a1c5-b8887447e56c/5177.fig.8.jpg)
Figure 8. Grain orientation maps of as-printed TiAl samples fabricated by different laser powers of (A) 230, (B) 290 and (C) 350 W.