Figure 5. Dilatometry curves of the sample length changes (strain) as a function of temperature for the as-fabricated FeCr0.4V0.3Ti0.2Ni1.3 high-entropy alloy at different rates of (A) 0.1 °C/s and (B) 10 °C/s.