Figure 6. Degradation kinetics of PXT (C0 = 20 µg/L) with TiO2 P-25 catalyst (200, 300, and 500 mg/L) under natural solar irradiation as a function of QUV (A) and t30W (B). PXT: Paroxetine.
Figure 6. Degradation kinetics of PXT (C0 = 20 µg/L) with TiO2 P-25 catalyst (200, 300, and 500 mg/L) under natural solar irradiation as a function of QUV (A) and t30W (B). PXT: Paroxetine.