A critical comparison of the main characterization techniques for microplastics identification in an accelerated aging laboratory experiment

Figure 2. (A) Raman spectra of the PE and PP polymer samples PE and PP correspond to the virgin samples and PE-d and PP-d correspond to the degraded samples after accelerated aging in the QUV; (B) corresponds to the prominence of the altered bands after accelerated aging. PE: Polyethylene; PP: polypropylene.