fig3
![An insight into the fate of Cu<sup>2+</sup> and zero-valent iron during removal of Cu<sup>2+</sup> by nanoscale zero-valent iron](https://image.oaes.cc/656444ff-dcc1-40d0-a095-1dbcf991a028/5578.fig.3.jpg)