fig5
![A lamellar-ordered poly[bi(3,4-ethylenedioxythiophene)-alt-thienyl] for efficient tuning of thermopower without degenerated conductivity](https://image.oaes.cc/fcf868be-a6b8-4452-b96f-756ec8df4dd0/5725.fig.5.jpg)
Figure 5. UV-vis absorption spectra of PBED, P(BED-T), P(BED-TT) films by spray-spin coating polymerization method. P(BED-TT) films. BED-T: 2,5-bis(2,3-dihydrothieno[3,4-b][1,4]dioxin-5-yl)thiophene; BED-TT: 2,5-bis(2,3-dihydrothieno[3,4-b][1,4]dioxin-5-yl)thieno[3,2-b]thiophene.