fig3
![Sulfur poisoning mechanism of LSCF cathode material in the presence of SO<sub>2</sub>: a computational and experimental study](https://image.oaes.cc/eb5e98f8-ad1b-47ce-b302-09a0d07771db/5486.fig.3.jpg)
Figure 3. SEM micro-image and the corresponding EDS mapping results of the selected region of heat-treated LSCF-6428 for 2 days under 10 ppm SO2 balanced with (A) dry air at 1,000 °C; (B) dry air at 800 °C, and (C) argon at 1,000 °C.
Figure 3. SEM micro-image and the corresponding EDS mapping results of the selected region of heat-treated LSCF-6428 for 2 days under 10 ppm SO2 balanced with (A) dry air at 1,000 °C; (B) dry air at 800 °C, and (C) argon at 1,000 °C.