Optimization strategies for high-performance aqueous zinc-sulfur batteries: challenges and future perspectives

Figure 5. (A) Schematic diagram of the function of the IL and LF-PLSD cathode. (B) The GCD plots of PLSD. (A and B) were cited with permission from Zhao et al.[42] Reproduction rights 2020, Wiley. (C) Experimental preparation process of ZnS@CF cathode. (D) The GCD plots of ZnS@CF. (C and D) were cited with permission from Liu et al.[53] Reproduction rights 2022, Elsevier. (E) Preparation scheme of Te1S7/C cathodes. (F) The working mechanism in Zn-Te1S7 batteries. (E and F) were cited with permission from Zhang et al.[73] Reproduction rights 2024, Wiley. (G) Experimental preparation process of ZnS1-xSex cathode. (H) The GCD profiles of batteries with ZnS and ZnS0.93Se0.07. (G and H) were cited with permission from Ren et al.[77] Reproduction rights 2024, Wiley.

Energy Materials
ISSN 2770-5900 (Online)
Follow Us

Portico

All published articles are preserved here permanently:

https://www.portico.org/publishers/oae/

Portico

All published articles are preserved here permanently:

https://www.portico.org/publishers/oae/