fig7
Figure 7. 18O2 pulse reaction over the (A) SrSnO3 and (B) Nd2Sn2O7 catalysts at 800 °C.
Figure 7. 18O2 pulse reaction over the (A) SrSnO3 and (B) Nd2Sn2O7 catalysts at 800 °C.