Influence of solid waste gypsum and additives on the properties of sulfoaluminate cement-fly ash-gangue ternary binder

Figure 3. The effect of gypsum on the strength of SAC-coal-based solid waste cementitious materials at (A) 1, (B) 3, (C) 7, and (D) 28 days. SAC: Sulfoaluminate cement.