Preparation and application of 0D, 2D and 3D molybdenite: a review

Figure 14. Schematic of MOCVD growth system (A)[67]. Raman spectrum of MoS2 films before (B1) and after (B2) sulfurization at 850 °C for 30 min (inset: SEM image of a triangular MoS2 domain following sulfurization). Schematic of 2D MoS2 synthesis (C). FTIR spectra of Na-DMDTC and Mo-DMDTC (D1). UV-vis absorbance (at 210 nm) of the mixture of Na-DMDTC and MoCl5 with varied molar ratios (d2). Optical image of 2D MoS2 (D3). AFM image of 2D MoS2 marked with a square box in (D4)[68].