Molecular dynamics simulations of nanoparticle sintering in additive nanomanufacturing: insights from sintering mechanisms

Figure 6. Distribution of GBs at the final sintering stage for 15 nm NPs with tilted misorientation angles of (A) 36.87o, (B) 53.15o for Ag NPs, and (C) 36.87o, (B) 53.15o for Cu NPs. Two sintering temperatures of 50%Tm and 70%Tm are included. The green arrows point to GBs. See Supplementary Materials for animations of selected key events. GBs: Grain boundaries; NPs: nanoparticles; Tm: bulk melting points.