fig25
![Numerical analysis on flow and surface topography of the molten pool in laser additive remanufacturing](https://image.oaes.cc/e7bfca6a-9e7d-42c7-8ca4-f638a46431fc/5915.fig.25.jpg)
Figure 25. Slag trajectory in the molten pool in the pulsed laser cladding at 0.540-0.542s.
Figure 25. Slag trajectory in the molten pool in the pulsed laser cladding at 0.540-0.542s.