fig4
Figure 4. (A) The electrical conductivity comparison of BZCYG4411 and other reported electrolytes; (B) Arrhenius plots of electrical conductivity of BZCYG4411 measured at 500-700 °C; (C) The TECs of BZCYG4411 and NiO-BZCYG4411 anode support measured at room temperature to 1,000 °C; (D) The linear shrinkages of the BZCYG4411 and NiO-BZCYG4411 versus temperature.