fig2

Combining ternary, ionic liquid-based, polymer electrolytes with a single-ion conducting polymer-based interlayer for lithium metal batteries

Figure 2. (A) Ionic conductivity of the TSPE in a temperature range of 30 to 100 °C; (B) Evolution of the viscoelastic parameters of the TSPE with temperature.