fig10

Figure 10. HRTEM images of (A) pristine MoS2 and (B) MoS2-CTAB; (C) In-situ SXRD tests of the MoS2-CTAB superstructure during the Zn2+ insertion/extraction processes; HRTEM images of MoS2-CTAB (D) after charging and (E) after discharging; (F) The electrochemical performance of the MoS2-CTAB superstructure under different mass loading[118]. Copyright 2022 American Chemical Society. HRTEM: High-resolution transmission electron microscopy; SXRD: synchrotron X-ray diffraction; CTAB: C19H42N+.