fig6

Unveiling the pattern and progression of reaction extent heterogeneity inside graphite electrodes through real-time monitoring of current density

Figure 6. (A-D) The comparison of current density and potential of layer 1 and layer 3 graphite electrodes during discharge at 0.1C, 0.2C, 0.33C, and 0.5C, respectively.