Unveiling the pattern and progression of reaction extent heterogeneity inside graphite electrodes through real-time monitoring of current density

Figure 5. (A-E) The current density distribution of four layers of graphite electrodes during discharge at 0.05C, 0.1C, 0.2C, 0.33C, and 0.5C, respectively; (F) The heterogeneity of SOC during discharge of graphite electrodes increases with the increment of cycling rate. SOC: State of charge.