Advancements in lithium solid polymer batteries: surface modification, <i>in-situ</i>/operando characterization, and simulation methodologies

Figure 11. (A) A structural model for NEMD simulations of the lithium/Xene (Xene = C, Si, Ge)/SPE interface. Temperature profiles of SPE at the interface, pristine sample (B) and with (C) graphene and (D) silicene. Reproduced with permission from Ref.[102] Copyright 2023, Elsevier. (E) Model of a symmetric solid-state lithium battery with two Li-metal electrodes, SSE, and current collectors. (F) Contact area ratio of electrodes with polymer electrolyte under varying pressures. Reproduced with permission from Ref.[103] Copyright 2022, Elsevier.