fig6
Figure 6. Galvanostatic cycling of two NMC-811||Li-Cu cells with QSPE-2 and QSPE-3 as electrolyte, coupled with EIS analysis. Galvanostatic cycling was performed at room temperature, in the voltage range between 3.0 and 4.3 V, and at constant C-rate of C/10 (with one initial cycle at C/20). The cathode active material loading was ~13 mg cm-2. EIS spectra were collected at the end of discharge, every