Figure 2. (A) LSV profiles of cc-Al||Li cells with different QSPEs, at 25 °C and 5 µV s-1; (B) floating current profiles of cc-Al||Li cells, with different QSPEs, collected at 25 °C and with step time of 10 h every 100 mV, between 3.8 and 5.0 V vs. Li/Li+.