fig6
Figure 6. (A) Cyclic test of pure LFP and LMC@3_1 cathodes under 1C charge and 10C discharge. (B) SEM images of pure LFP electrode after cyclic test. (C) SEM images of LMC@3_1 electrode after cyclic test. Heat map of original in-situ XRD patterns under 2C charge/discharge for (D) pure LFP and (E) LMC@3_1 electrodes after cyclic test.