fig7
Figure 7. SEM images of LMAs disassembled from Li||LRM cells after 200 cycles with (A) BE and (C) B-0.5 electrolytes, wherein (B) and (D) are the corresponding locally enlarged images. SEM images of LRM particles after 200 cycles in (E) BE and (F) B-0.5 electrolytes. XPS spectra of the cycled LRM cathodes in (G-I) BE and (J-L) B-0.5 electrolytes.