fig1
Figure 1. (A) Optical photos of the laser beam passing through BE. (B-D) Laser beam passing through (B) upper, (C) middle and (D) lower parts of B-0.5. (E) Oxidation and (F) reduction stability of BE and B-0.5 by LSV at a scan rate of 0.5 mV s-1.