fig1
Figure 1. Cycling performance of the Zn||Zn symmetric cells using three hybrid electrolytes. Galvanostatic Zn plating/stripping under 1mA cm-2 and 0.5 mAh cm-2 at (A) 30 °C and (B) 60 °C; Galvanostatic Zn plating/stripping under different current densities and 0.5 mAh cm-2 capacity in (C) G4-based; (D) PC-based; and (E) DMF-based hybrid electrolytes at 60 °C. PC: Propylene carbonate; DMF: Dimethylformamide.