fig3

Promoted de-solvation effect and dendrite-free Zn deposition enabled by <i>in-situ</i> formed interphase layer for high-performance zinc-ion batteries

Figure 3. Bare Zn and V2O5-x protective layer V@Zn after 1, 5 and 10 min reaction, respectively. (A-C) Thickness of the V2O5-x interface layer; (D) the magnified voltage-time profiles from 200 h to 210 h; (E) long cycle stability testing; (F) contact angle measurement.