fig8

Figure 8. (A) J-V curves of ZnIn2S4, Mg:ZnIn2S4, Co:ZnIn2S4 and Mg:ZnIn2S4/Co:ZnIn2S4 homojunction photoanodes measured in 0.2 M Na2SO4 solution under AM 1.5G illumination; (B) J-t curves measured at 1.23 V vs. RHE under chopped simulated sunlight illumination with 30 s light on/off cycles; (C) Schematic diagram of Mg:ZnIn2S4/Co:ZnIn2S4 photoanode to enhance the photoelectric performance by enhancing the separation of bulk and interface charges[79]. Copyright 2021, Elsevier. J-V: Photocurrent density-voltage; J-t: transient photocurrent density; RHE: reversible hydrogen electrode.