fig8
![Recent advances of cobalt-free and nickel-rich cathode materials for lithium-ion batteries](https://image.oaes.cc/c0604cec-0234-4a05-97cb-d494a45febbf/em4008.fig.8.jpg)
Figure 8. (A) Schematic illustration for the mechanism of single crystal structure mitigating the structure degradation and performance deterioration of LiNi0.9Mn0.1O2 (NM91), (B and C) SEM images of PC-NM91 (B) and SC-NM91 (C), (D) Half-cell cycling tests of