fig1

Guiding lithium growth direction by Au coated separator for improving lithium metal anode

Figure 1. Schematic illustration of lithium depositing on (A) Cu and (B) AuPP. (C) Optical images of cross-section view of the simulated cell after lithium depositing for 0, 15 and 20 min. (D) Calculated binding energy of a lithium ion with Cu and Au. The contact angles of molten lithium with (E) Cu and (F) Au.