fig6
![Layer-by-layer assembling redox wood electrodes for efficient energy storage](https://image.oaes.cc/df96c223-835f-45bf-9387-f2cec4c935cb/em3096.fig.6.jpg)
Figure 6. (A-C) TEM and EDS analysis of PPy nanostructure, after scratching powder from PPy@TrW electrode. (D-F) TEM and EDS analysis of PPy@CNTs nanostructure, after scratching powder from PPy@CNTs@TrW electrode. (G) FTIR plots in 850-1,800 cm-1 region for PPy@TrW and PPy@CNTs@TrW. (H) XRD plots of TrW, PPy@TrW and PPy@CNTs@TrW.