fig4
![<i>In-situ</i> Li<sub>2</sub>O-atmosphere assisted solvent-free route to produce highly conductive Li<sub>7</sub>La<sub>3</sub>Zr<sub>2</sub>O<sub>12</sub> solid electrolyte](https://image.oaes.cc/c0d05576-eb33-4e7b-940f-28a099a5da81/em4087.fig.4.jpg)
Figure 4. Cross-section SEM images of the Li0L0 and Li0L4 pellets sintered at (A) 1,220 °C × 20 min, (B) 1,260 °C × 20 min.
Figure 4. Cross-section SEM images of the Li0L0 and Li0L4 pellets sintered at (A) 1,220 °C × 20 min, (B) 1,260 °C × 20 min.