fig1
![<i>In-situ</i> Li<sub>2</sub>O-atmosphere assisted solvent-free route to produce highly conductive Li<sub>7</sub>La<sub>3</sub>Zr<sub>2</sub>O<sub>12</sub> solid electrolyte](https://image.oaes.cc/c0d05576-eb33-4e7b-940f-28a099a5da81/em4087.fig.1.jpg)
Figure 1. Phase result of sintered powders. XRD patterns of as-calcinated Li6Zr2O7 and Li0 via wet and dry routes.
Figure 1. Phase result of sintered powders. XRD patterns of as-calcinated Li6Zr2O7 and Li0 via wet and dry routes.
All published articles are preserved here permanently:
https://www.portico.org/publishers/oae/