fig5
![Strategies towards inhibition of aluminum current collector corrosion in lithium batteries](https://image.oaes.cc/1fd2b517-857b-4513-9f93-8fed817343cc/em3053.fig.5.jpg)
Figure 5. (A) Design of the fluorinated cyclic phosphate solvent. (B) High-resolution XPS spectra of the Al foil after the chronoamperometry tests carried out in the three electrolytes: Al 2p (left column), F 1s (middle column), and P 2p (right column).