![Evaluation of asymmetric poly(vinylidene fluoride)-coated polyimide separator with three-dimensionally homogeneous microporous structure for high-safety lithium-ion battery](https://image.oaes.cc/b8ed5c91-a6ff-46da-8157-7457583821ac/em30143.fig.3.jpg)
Figure 3. Surface and cross-sectional SEM images of 3DHM API/PVDF separator (A) the unmodified side, (B and C) the modified side, (D) the upper section, (E) the overall cross-section and (F) the lower section.