![Quasi-solid-state electrolytes - strategy towards stabilising Li|inorganic solid electrolyte interfaces in solid-state Li metal batteries](https://image.oaes.cc/7a51a42f-906c-4abd-bd6e-0e8984716874/5603.fig.2.jpg)
Figure 2. (A) Schematic open-circuit energy diagram for a Li|SSE|LixMyO2 battery system where μLi and μLixMyO2 represent the chemical potentials of Li and the cathode materials, respectively. Reprinted (adapted) with permission from Pervez et al.[95]. Copyright (2019) American Chemical Society. (B) Schematic band diagrams of the HOMO and LUMO of different classes of electrolytes. Reprinted (adapted) with permission from Banerjee et al.[97]. Copyright (2020) American Chemical Society. (C) The interphase formed between SSE and lithium metal with (a) thermodynamically stable two-dimensional interphase, (b) mixed ionic-electronic conducting interphase (MCI) formed due to thermodynamic instability of SSE with lithium, and (c) growth of stable three-dimensional interphase due to the poor electronic conductive reaction products. This figure is reproduced with permission from Wenzel et al.[98].