fig3
![Air-exposed lithium metal as a highly stable anode for low-temperature energy storage applications](https://image.oaes.cc/69e10192-18fd-47fe-9176-4c0455e8a3dd/5311.fig.3.jpg)
Figure 3. (A) EIS plots, (B) Rct variations after cycling, (C) Tafel plots and (D) exchange current density variations after cycling of pure Li, Li-10 min, Li-30 min, Li-1 h and Li-2 h. (E) Corresponding voltage-time profiles of Li plating/stripping at current densities of 1, 2, 3, 5 and 10 mA cm-2 in symmetrical cells. (F) Long cycling voltage-time profiles at 1 mA cm-2. Insets show selected voltage-time profiles.