fig4

Constructing stable lithium metal anodes using a lithium adsorbent with a high Mn<sup>3+</sup>/Mn<sup>4+</sup> ratio

Figure 4. (A) Cross-sectional SEM images of HMO-5-coated separator after Li electroplating of 2 and 4 mAh cm-2. (B) top-view SEM images of Li deposits on HMO-coated-Cu electrodes after Li electroplating of 4 mAh cm-2.