fig8
Figure 8. Radial displacement of PEEK 450G stent (Left) with artery (Right) at non-plaque (A) and plaque (B) regions when subjected to 0.8 MPa pressure load. PEEK: polyether ether ketone
Figure 8. Radial displacement of PEEK 450G stent (Left) with artery (Right) at non-plaque (A) and plaque (B) regions when subjected to 0.8 MPa pressure load. PEEK: polyether ether ketone